Page 3 of 3

Re: Hard soldering. Brazing. Silver.

PostPosted: Mon Sep 05, 2016 10:46 am
by WTDist
lol, i will go there and get them in my high vis too then :))
even though i dont work anymore :))

thats a good price

Re: Hard soldering. Brazing. Silver.

PostPosted: Mon Sep 05, 2016 11:05 am
by P3T3rPan
WTDist wrote:Couple of questions though,

when brazing does it help to clean the joints with some sand paper or something like with soft solder?
Copper self cleans when up to dull red then left for a couple of moments to go black(cool). Only the worst lead based paint can be difficult but I guess you wont be using that shit. Some "sandpapers" leave shit on the join area causing grieff

and i know people say you dont need flux with copper to copper and i did not use any this time or when i do flange rings but is there any benefit for it with flux on copper to make it a little easier or is it just a waste of time and money?
I do this for a living and only use flux when brazing dissimilar metals (brass to copper etc) cos it is a waste of money and flux deposits cause corrosion in the long term and/or hide defects in the short term

and lastly i used 2% a while ago on rings for flanges and switched to 5% (used this today also) and saw a msssive difference in how easy it was to use compared to the 2% on the swivel map gas torch. Does the silver % matter just as much now i have the oxy/map kit with the high heat?

The higher the silver the less heat is needed. This can be exploited when doing lots of joins in close proximity. For example shotgun condensers
Your best friend when doing pretty joins is whiteout
After many years soldering stuff as an apprentice we started brazing using silver alloys and threw all our problems away with the soldering gear

Re: Hard soldering. Brazing. Silver.

PostPosted: Mon Sep 05, 2016 11:26 am
by WTDist
cheers p3t3r, that helps alot

Re: Hard soldering. Brazing. Silver.

PostPosted: Mon Sep 05, 2016 11:27 am
by P3T3rPan
goes black
IMG_3287.JPG

White out
IMG_3286.JPG

no flux (No cleanup done on this)
IMG_3299 (640x480).jpg

Re: Hard soldering. Brazing. Silver.

PostPosted: Thu Nov 30, 2017 4:30 pm
by bluc
So for silver soldering(not soft solder) what flux do i need for copper to stainless?

Re: Hard soldering. Brazing. Silver.

PostPosted: Thu Nov 30, 2017 6:16 pm
by bluc
So after spending last 2ish hours on the topic I have bought some stay silv by harris. Good for high temp silver soldering stainless to copper :handgestures-thumbupleft:

Re: Hard soldering. Brazing. Silver.

PostPosted: Thu Nov 30, 2017 7:01 pm
by P3T3rPan
bluc wrote:So for silver soldering(not soft solder) what flux do i need for copper to stainless?

Well I used this cos that is what I have and am used to.
flux.JPG

Now i use this. :cool:
TIG.JPG